WE HAVE SOME GREAT LIMITED-TIME OFFERS - CLICK HERE TO VIEW THEM WE SHIP WORLDWIDE    /    All UK ORDERS GREATER THAN £75 EX VAT DELIVERED FREE    /    WE SHIP WORLDWIDE    /    ALL EUROPEAN ORDERS GREATER THAN £500.00 ex VAT DELIVERED FREE    /    WE SHIP WORLDWIDE
    Share this page on Facebook   Share this page on LinkedIn   Share this page on Twitter   Share this page on Whatsapp   

    Rapid Ref : RX431500  

    SIF SILVER SOLDER No 43, 1.5mm Brazing Wire, 1Kg Pack - EN ISO 17672: AG 155, EN 1044: AG 103, BS 1845: AG 14
    RX431500

    Contact Us For Price 

    Cadmium Free 55% Silver Solder, which is free flowing and ideal for close-fitting capillary joints and for a colour match on stainless. Use with SIF SILVER SOLDER flux.

    EN ISO 17672 Ag 155
    EN 1044: AG 103, BS: 1845 AG14

    Metal Composition%: 55 Ag, 21 Cu, 22 Zn, 2 Sn
    Melting: 630 - 660°c
    U.T.S N/mm²: 415
    Hardness BHN: 145

    Brochures & Manuals

    BROCHURES & MANUALS
       View Brochure

    Related Items

    Silver (Ag) FAQs

    Straight answers to the questions people ask most when choosing and using silver brazing rods and wire.

    What does the silver percentage in a brazing alloy tell me?icon-minus-redicon-plus-red

    It tells you roughly what sort of alloy it is. Silver brazing alloys range from fairly low to high silver content, and the balance is mainly copper and zinc, sometimes with a little tin or nickel. The silver content affects colour, melting range and how freely the filler flows.

    As a general guide, higher silver alloys are whiter and tend to run at lower temperatures and flow more freely into tight joints, while lower silver alloys look more yellow, like brass. The exact melting range and best joint gap are different for every alloy, so read the maker's data sheet rather than relying on the percentage alone.

    Why choose a cadmium-free silver brazing alloy?icon-minus-redicon-plus-red

    Older silver brazing alloys often contained cadmium, which gives off highly toxic cadmium oxide fume when it is heated, and overheating makes this worse. The HSE has guidance for people using cadmium-containing brazing products, and serious illness has been recorded after exposure to the fume.

    Cadmium-free alloys remove that particular hazard and are the usual choice today. You still need good ventilation or local extraction for the flux and metal oxide fume, and you should be careful with any cadmium plating on the parts, which should be dealt with before heating. Follow the maker's safety data sheet and your risk assessment.

    Should I buy bare rod or flux-coated rod?icon-minus-redicon-plus-red

    Bare rod is used with flux applied separately, as a paste or powder mixed with water, which lets you place the flux exactly where it is needed and choose a flux to suit the job. Flux-coated rod carries the flux on the outside, so you do not have to apply it by hand, which is convenient for site and repair work and for awkward positions.

    The coating suits many jobs, but where you need a specific type of flux, such as for stainless steel or long heating cycles, bare rod with a chosen flux is often the better route. Check the maker's data sheet for the flux type.

    How big should the joint gap be for silver brazing?icon-minus-redicon-plus-red

    Very small. Silver brazing relies on capillary action, which draws the molten filler into a narrow gap, so the parts should fit closely with only a fraction of a millimetre between them. Too wide a gap weakens the joint and can leave voids, while no gap at all stops the filler entering.

    The best gap is the one at brazing temperature, not room temperature, and it changes if the two metals expand at different rates. The maker's data sheet gives the recommended gap for each alloy, so use that figure.